High temperature oxidation of AISI 441 in simulated solid oxide fuel cell anode side conditions
Artikel i vetenskaplig tidskrift, 2022

This study investigates the corrosion of AISI 441 in simulated anode conditions of solid oxide fuel cells (SOFCs). Several parameters such as temperature, humidity, surface condition, pre-oxidation temperature and environment, were investigated. Samples pre-oxidized at 800 ºC were protective at 550–900 ºC, while as-received samples showed protective behavior only at 900 ºC. Additional exposures performed at 600 ºC revealed the negative effect of increasing steam concentration, the beneficial effect of grinding, while pre-oxidation at 600 ºC did not improve the protectiveness. The role and the interplay of the aforementioned factors are discussed.

Solid oxide fuel cells

Hydrogen

AISI 441

Water vapor

Interconnect

Anode side

Författare

Anton Chyrkin

Chalmers, Kemi och kemiteknik, Energi och material

Kerem Gündüz

Chalmers, Kemi och kemiteknik, Energi och material

Gebze Teknik Üniversitesi (GYTE)

Vijayshankar Asokan

Chalmers, Kemi och kemiteknik, Energi och material

Jan-Erik Svensson

Chalmers, Kemi och kemiteknik, Energi och material

Jan Froitzheim

Chalmers, Kemi och kemiteknik, Energi och material

Corrosion Science

0010-938X (ISSN)

Vol. 203 110338

Ämneskategorier

Annan kemi

Metallurgi och metalliska material

Korrosionsteknik

DOI

10.1016/j.corsci.2022.110338

Mer information

Senast uppdaterat

2022-05-19