For Intermediate-Temperature SOFC, the lower operating temperature allows for a broader range of steel grades to be used as interconnects. This work compares the oxidation performances of six Cr2O3-forming steels and one Al2O3-forming steel, under single- and dual-atmosphere conditions. Single-atmosphere exposures in combination with Cr(VI) evaporation measurements were carried out at 600 °C. Except for AISI 430 all the Cr2O3-forming steels showed protective behaviour with similar Cr(VI) evaporation values and low area specific resistance (ASR) values. Kanthal EF101 showed the lowest level of Cr(VI) vaporisation but substantially higher ASR values. Dual-atmosphere exposures were carried out at 600 °C in Ar-5%H2–3%H2O//air-3%H2O. All Cr2O3-forming steels suffered various degrees of breakaway corrosion. Therefore, operation under dual-atmosphere conditions is likely the life-time-limiting failure mode.

Corrosion

Dual-atmosphere

Laves phases

Interconnect

Cr(VI) evaporation

IT-SOFC

Författare

Matthieu Tristan Tomas

Chalmers, Kemi och kemiteknik, Energi och material

Jan-Erik Svensson

Chalmers, Kemi och kemiteknik, Energi och material

Jan Froitzheim

Chalmers, Kemi och kemiteknik, Energi och material

International Journal of Hydrogen Energy

0360-3199 (ISSN)

Vol. 65 112-125

Utveckla kostnadseffektiva metalliska material för fastoxidceller för ett elektrifierat samhälle

VINNOVA (2021-01003), 2021-05-01 -- 2024-08-31.

Ämneskategorier

Korrosionsteknik

DOI

10.1016/j.ijhydene.2024.04.010

Mer information

Senast uppdaterat

2024-06-12